Material Notes:
Typical Applications: Electrical partsUL94 V-0 Flame RetardantInformation provided by PTS LLC.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Water Absorption 0.10 %

@Temperature 23.0 °C,
Time 86400 sec
0.10 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 300 °C
50 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.0 MPa
7540 psi
type I; ASTM D638
Elongation at Break 30 %
30 %
type I; ASTM D638
Flexural Strength 85.0 MPa
12300 psi
2.6 mm/min; ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
2.6 mm/min; ASTM D790
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.40 mm
212 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in