PSM Industries Ferro-TiC® HT-6A Age Hardenable Nickel Base

Category Ceramic , Carbide , Metal , Nonferrous Metal , Nickel Alloy
Manufacturer PSM Industries
Trade Name Ferro-TiC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Ferro-TiC® HT-6A Age Hardenable Nickel Base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Excellent oxidation and corrosion resistance at high temperatures. Replaces Stellite™/Inconel™. Non-magnetic.Ferro-TiC® Unique CharacteristicsProvides the lightweight, size, stability, and hardnessVirtually porosity free - significantly better than the A1 ASTM B-276-79 StandardLow specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide10 times the wear resistance of tool steelsEconomical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)50-90% less linear size change in heat treat than tool steelsInformation Provided by Ferro-TiC®, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.80 g/cc
0.246 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 46
46
Annealed
52
52
Hardened
Flexural Strength 1320 MPa
191000 psi
Transverse Rupture
Compressive Strength 1970 MPa
285000 psi
Charpy Impact Unnotched 5.36 J/cm²
25.5 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear 8.87 µm/m-°C

@Temperature 21.1 - 982 °C
4.93 µin/in-°F

@Temperature 70.0 - 1800 °F
Maximum Service Temperature, Air 982 °C
1800 °F
Descriptive Properties Value Comments
Carbide (Vol. %) 40
Linear Size Change Thru Heat Treat % -0.014
Thermal Shock (No. Cycles) 11