Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 0.0167 - 43200 min
0.000278 - 720 hour
Average value: 492 min Grade Count:280
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Cure Time 0.0167 - 0.0333 min
0.000278 - 0.000556 hour
Rubber set time
Lord Adhesives 8300 Medium Setting, Medium Viscosity Ethyl Cyanoacrylate Adhesive
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal..
Cure Time 0.0167 min
0.000278 hour
400 W/inch @ 1"
Tra-Con Tra-Bond F175T One-Part Thixotropic UV Curing Adhesive
TRA-BOND F175T is a thixotropic, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure w..
Cure Time 0.0167 min
0.000278 hour
400 W/inch @ 1"
Tra-Con Tra-Bond F175 One-Part UV Curing Adhesive
TRA-BOND F175 is a clear, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure with ult..
Cure Time <= 0.0167 min
<= 0.000278 hour
Dymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic Bonder
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic BonderExcellent adhesion to plastics, glass, met..
Cure Time <= 0.0167 min
<= 0.000278 hour
Dymax Ultra Fast™ 3-3094 Plastic Bonding Adhesive
Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and TerminatingCost EffectiveUltra Light-Weld® UV/Visible adhesives set in as little as one secondOn a material cost per applica..
Cure Time <= 0.0167 min
<= 0.000278 hour
Dymax Ultra Fast™ 3-3095 Tack Gel Adhesive
Ultra Fast™ Adhesives for Wire Harness, Strain Relief, Coil Coating and TerminatingCost EffectiveUltra Light-Weld® UV/Visible adhesives set in as little as one secondOn a material cost per applica..
Cure Time 0.0167 - 0.167 min
0.000278 - 0.00278 hour
Time to Handling
3M Scotch-Weld™ MG05 PR Medical Grade Instant Adhesive
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti..
Cure Time 0.0167 - 0.167 min
0.000278 - 0.00278 hour
Time to Handling Strength
3M Scotch-Weld™ PR5 Plastic and Rubber Instant Adhesive
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates ..
Cure Time <= 0.0167 min
<= 0.000278 hour
Dymax 9-3095-Gel Strain Relief, Wire and Parts Tacking Adhesive
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-3095-Gel Strain Relief, Wire and Parts Tacking AdhesiveFor fastest curing, cure with UV and visible light Cure Typ..