Omni Plastics OmniTuff™ HPP GRC10 Homopolymer Polypropylene Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Omni Plastics
Trade Name OmniTuff™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Omni Plastics OmniTuff™ HPP GRC10 Homopolymer Polypropylene Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Flexural Modulus 2.56 GPa
372 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256