Material Notes:
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extraction by blood lipids and high fat emulsions. This family of compounds is designed to be molded or extruded, whichever is required. Colorite 77 compounds are available in a range of hardnesses from flexible to semi-rigid. They are also available in ethylene oxide and radiation sterilizable grades. As with all Colorite non-toxic compounds, traceability and lot identification of all raw materials and finished products are maintained. Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 17.9 MPa
2600 psi
ASTM D638
Elongation at Break 375 %
375 %
ASTM D638
100% Modulus 0.009825 GPa
1.425 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D746