Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Niche Polymer PA66MI40BK Nylon 66, 40% Mineral Fiber Filled, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled , Nylon 66, Impact Grade
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PA66MI40BK Nylon 66, 40% Mineral Fiber Filled, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00900 cm/cm
0.00900 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 101 MPa
14600 psi
ASTM D638
Elongation at Break 6.00 %
6.00 %
ASTM D638
Flexural Modulus 4.50 GPa
653 ksi
ASTM D790
Izod Impact, Unnotched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 249 - 260 °C
480 - 500 °F
ASTM D789
Descriptive Properties Value Comments
Color Black