Material Notes:
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Thermal Properties Metric English Comments
Melting Point 1135 - 1169 °C
2075 - 2136 °F
Solidus 1135 °C
2075 °F
Liquidus 1169 °C
2136 °F
Component Elements Properties Metric English Comments
Gold, Au 30 %
30 %
Nickel, Ni 36 %
36 %
Palladium, Pd 34 %
34 %