Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.958 - 0.962 g/cc
0.0346 - 0.0348 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.60 - 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 - 0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
30 - 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 - 40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 50; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.40 GPa
>= 203 ksi
ASTM D790
Izod Impact, Notched >= 1.60 J/cm

@Temperature 23.0 °C
>= 3.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: