NCMT NanoPAC™ G3000 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ G3000 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automobile Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
NCMT Method
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Tensile Modulus 6.00 GPa
870 ksi
ASTM D638
Izod Impact, Notched 0.540 J/cm
1.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temp.; ASTM D648