Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0067 cm/cm
0.0067 in/in
ASTM D955-89
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 46.9 MPa
6800 psi
ASTM D638-95
Elongation at Break 21 %
21 %
ASTM D638-95
Flexural Strength 65.9 MPa
9560 psi
ASTM D790-95
Flexural Modulus 0.250 GPa
36.3 ksi
ASTM D790-95
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256-93a
Gardner Impact 1.70 J
1.25 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648-95