Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flamâ„¢ 0801 LDPE Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Multibase
Trade Name Multi-Flam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flamâ„¢ 0801 LDPE Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 0.224 GPa
32.5 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.0313 in
V-0
V-0
0.125 in