ChevronTexaco Clarity® ISO 320 Paper Machine Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Clarity®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Clarity® ISO 320 Paper Machine Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOSYN® base stocks. Their ashless extreme pressure additive packages include rust, oxidation, and foam inhibitors. Their outstanding oxidation stability minimizes deposit formation.These oils have gear oil EP characteristics to minimize wear, and yet do not contain corrosive active sulfur additives. The ashless formulations facilitate reclaiming and recycling of circulating oils.They have excellent water separating ability (demulsibility), and also have superior wet filterability with fine porosity oil filters, as demonstrated by the Pall Filterability Test.ApplicationsThe Chevron Clarity Paper Machine Oil series is recommended for use in all circulating systems of paper machines, including wet-end systems, dryer bearings, and calender stacks.Chevron Clarity Paper Machine Oils have been used successfully in the lubrication of many types of paper machine equipment including Valmet, Beloit, and Voith Sulzer paper machine equipment.In addition, Chevron Clarity Paper Machine Oils exceed the best of the competition in the Pall Filterability Test using low micron filters.Chevron Clarity Paper Machine Oils ISO 100, 150, 220, 320, and 460 may be used as AGMA EP Oils 3, 4, 5, 6, and 7, respectively, for back-side gears and enclosed gear drives. Chevron Clarity Paper Machine Oils ISO 220 and 320 may also be used in plain and antifriction bearings.
Physical Properties Metric English Comments
API Gravity 26.1 °
26.1 °
Viscosity Measurement 98
98
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1616 SUS
1616 SUS
Saybolt Viscosity at 210°F 117 SUS
117 SUS
Kinematic Viscosity at 40°C (104°F) 304 cSt
304 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 23.5 cSt
23.5 cSt
ASTM D445
Oxidative Stability 3000 hour
3000 hour
Mechanical Properties Metric English Comments
Timken Test 27200 g
60.0 lb
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 248 °C
478 °F
ASTM D92
Descriptive Properties Value Comments
FZG Gear Wear Test, Failure Load Stage 13
Pall Filterability, Wet aged, mL to 25 psi >17000
Rust preventative Test Procedure B Pass
Synthetic Sea Water