| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant |
| Manufacturer | Multibase |
| Trade Name | Multi-ABS |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Multibase Multi-ABS 2925 FR Flame Retardant ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.21 g/cc | 0.0437 lb/in³ | ASTM D792-91 |
| Melt Flow | 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238-94a |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM D638-95 |
| Elongation at Break | 30 % | 30 % | ASTM D638-95 |
| Flexural Modulus | 2.00 GPa | 290 ksi | RT; ASTM D-790-95 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 161 °C | 322 °F | injection molded unannealed; ASTM D-648-95 |
| 195 °C | 383 °F | compression molded annealed; ASTM D-648-95 | |
| 196 °C | 385 °F | injection molded annealed; ASTM D-648-95 | |
| Vicat Softening Point | 99.0 °C | 210 °F | ASTM D1525-95 |
| Flammability, UL94 | V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
5V |
| V-0 @Thickness 1.59 mm |
V-0 @Thickness 0.0625 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 35.4 kV/mm | 899 kV/in | ASTM D149-95 |