Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials IS802 White Adhesive Sealant, General Purpose Paste

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials IS802 White Adhesive Sealant, General Purpose Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose, cost-effective sealing and bonding. Cure-in-place electrical insulation. UL approval.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 23
23
Tensile Strength, Ultimate 2.06 MPa
299 psi
Elongation at Break 450 %
450 %
Adhesive Bond Strength 0.970 MPa
141 psi
Typical lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Continuous useful temperature.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Dielectric Constant 2.9

@Frequency 60 Hz
2.9

@Frequency 60 Hz
Dielectric Strength 20.0 kV/mm
508 kV/in
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F