Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mikro-Technik Mikrolen AST UHMW-PE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Mikro-Technik
Trade Name Mikrolen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mikro-Technik Mikrolen AST UHMW-PE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Antistatic ModifiedProperties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -265°C up to +80°C (100°C) in relation to mechanical stressInformation provided by Mikro-Technik GmbH
Physical Properties Metric English Comments
Density >= 0.960 g/cc
>= 0.0347 lb/in³
Mechanical Properties Metric English Comments
Ball Indentation Hardness 38.0 MPa
5510 psi
30 sec
Tensile Strength, Yield >= 40.0 MPa
>= 5800 psi
Elongation at Break >= 300 %
>= 300 %
Izod Impact, Notched (ISO) >= 130 kJ/m²
>= 61.9 ft-lb/in²
double notch
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+6 ohm-cm
<= 1.00e+6 ohm-cm
Surface Resistance <= 1.00e+9 ohm
<= 1.00e+9 ohm
Descriptive Properties Value Comments
Tensile E-modulus 8.4