Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 20 - 50
20 - 50
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Tensile Strength, Yield 60.0 - 210 MPa
8700 - 30500 psi
Elongation at Break 20 - 35 %
20 - 35 %
Modulus of Elasticity 138 GPa
20000 ksi
Machinability 40 %
40 %
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 240 W/m-K
1670 BTU-in/hr-ft²-°F
Melting Point 1040 - 1080 °C
1900 - 1980 °F
Solidus 1040 °C
1900 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.20 - 0.60 %
0.20 - 0.60 %
Copper, Cu 98 %
98 %
as balance
Nickel, Ni 1.4 - 2.2 %
1.4 - 2.2 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000570 - 0.00000860 ohm-cm
0.00000570 - 0.00000860 ohm-cm
20-30% IACS Conductivity