Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30N 44-51Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 23 - 30
23 - 30
Hardness, Vickers 250 - 301
250 - 301
Tensile Strength, Ultimate 820 - 940 MPa
119000 - 136000 psi
Tensile Strength, Yield 650 - 870 MPa
94300 - 126000 psi
Elongation at Break 12 - 22 %
12 - 22 %
Modulus of Elasticity 131 GPa
19000 ksi
Fatigue Strength 290 - 330 MPa

@# of Cycles 1.00e+8
42100 - 47900 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 200 °C
9.44 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K
729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C
1600 - 1800 °F
Solidus 870 °C
1600 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.8 - 2.0 %
1.8 - 2.0 %
Co + Ni >= 0.20 %
>= 0.20 %
Co + Ni + Fe <= 0.60 %
<= 0.60 %
Copper, Cu 98 %
98 %
as balance
Lead, Pb <= 0.020 %
<= 0.020 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm
0.00000610 - 0.0000101 ohm-cm
17-28% IACS Conductivity