Category | Ceramic , Sulfide/Chalcogenide , Other Engineering Material , Semiconductor |
Manufacturer | Mateck GmbH |
Trade Name | |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Mateck Zinc Sulfide Cleartran (ZnS).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.09 g/cc @Temperature 20.0 °C |
0.148 lb/in³ @Temperature 68.0 °F |
|
Solubility | 0.000065 ppm | 0.000065 ppm | |
Molecular Weight | 97.43 g/mol | 97.43 g/mol |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Vickers Microhardness | 14.7 | 14.7 | MPa |
Modulus of Elasticity | 74.5 GPa | 10800 ksi | |
Poissons Ratio | 0.28 | 0.28 | |
Shear Modulus | 29.1 GPa | 4220 ksi | Calculated |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 µm/m-°C @Temperature -60.0 - 60.0 °C |
3.61 µin/in-°F @Temperature -76.0 - 140 °F |
|
Specific Heat Capacity | 0.515 J/g-°C | 0.123 BTU/lb-°F | |
Thermal Conductivity | 27.2 W/m-K @Temperature 38.0 °C |
189 BTU-in/hr-ft²-°F @Temperature 100 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 2.20084 | 2.20084 | at n10.0 |
2.44915 | 2.44915 | at n0.4678 | |
2.15252 @Wavelength 13000 nm |
2.15252 @Wavelength 13000 nm |
||
2.24661 @Wavelength 5000 nm |
2.24661 @Wavelength 5000 nm |
||
2.31669 @Wavelength 780 nm |
2.31669 @Wavelength 780 nm |
||
2.48918 @Wavelength 435.8 nm |
2.48918 @Wavelength 435.8 nm |
||
Transmission, Visible | 60 % @Wavelength 500 nm |
60 % @Wavelength 500 nm |
Internal Transmittance |
IR Transmittance | 5.0 % @Wavelength 15000 nm |
5.0 % @Wavelength 15000 nm |
Internal Transmittance |
70 % @Wavelength 10000 nm |
70 % @Wavelength 10000 nm |
Internal Transmittance | |
UV Transmittance | 9.0 % @Wavelength 350 nm |
9.0 % @Wavelength 350 nm |
Internal Transmittance |
Descriptive Properties | Value | Comments |
---|---|---|
Syngony | cubic | |
Thermal Coefficient of Refractive Index | 5.43E-05 | at 0.6328 microns |
Transmission Range (microns) | 0.37 - 14 |