Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mateck Gallium Arsenide (GaAs)

Category Ceramic , Phosphide/Pnictide , Other Engineering Material , Semiconductor
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck Gallium Arsenide (GaAs).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Optical crystals
Physical Properties Metric English Comments
Density 5.316 g/cc

@Temperature 20.0 °C
0.1921 lb/in³

@Temperature 68.0 °F
Solubility 0.00 ppm
0.00 ppm
a Lattice Constant 5.653 Ã…
5.653 Ã…
Molecular Weight 144.64 g/mol
144.64 g/mol
Mechanical Properties Metric English Comments
Vickers Microhardness 6900
6900
MPa
Hardness, Mohs 4.5
4.5
Modulus of Elasticity 85.0 GPa
12300 ksi
Poissons Ratio 0.31
0.31
Shear Modulus 32.4 GPa
4700 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 5.39 µm/m-°C

@Temperature 0.000 - 30.0 °C
2.99 µin/in-°F

@Temperature 32.0 - 86.0 °F
Specific Heat Capacity 0.350 J/g-°C
0.0837 BTU/lb-°F
Thermal Conductivity 46.05 W/m-K

@Temperature 25.0 °C
319.6 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Melting Point 1238 °C
2260 °F
Optical Properties Metric English Comments
Refractive Index 3.34
3.34
n8.0
2.41

@Wavelength 19000 nm
2.41

@Wavelength 19000 nm
2.82

@Wavelength 14500 nm
2.82

@Wavelength 14500 nm
3.34

@Wavelength 8000 nm
3.34

@Wavelength 8000 nm
IR Transmittance 1.0 %

@Wavelength 900 nm
1.0 %

@Wavelength 900 nm
Internal Transmittance
2.0 %

@Wavelength 15000 nm
2.0 %

@Wavelength 15000 nm
Internal Transmittance
55 %

@Wavelength 1500 nm
55 %

@Wavelength 1500 nm
Internal Transmittance
60 %

@Wavelength 10000 nm
60 %

@Wavelength 10000 nm
Internal Transmittance
Descriptive Properties Value Comments
Absorption loss (cm^-1) 0.26
at 8.0 microns
Symmetry Class 43m F43m
Syngony cubic
Transmission Range (microns) 1 - 15
Users viewing this material also viewed the following: