Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP3SP5FL High Shear and High Peel Strength One Component Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP3SP5FL High Shear and High Peel Strength One Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
“Snap” cure version of EP3FL. Fastest curing system available. Ideal for high speed manufacturing & production. Good physical properties. Bonds well to most substrates.
Physical Properties Metric English Comments
Viscosity 80000 - 90000 cP

@Temperature 23.0 °C
80000 - 90000 cP

@Temperature 73.4 °F
Storage Temperature 23.9 °C
75.0 °F
6 weeks
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 0.330 min

@Temperature 204 °C
0.00550 hour

@Temperature 400 °F
0.960 min

@Temperature 149 °C
0.0160 hour

@Temperature 300 °F
Descriptive Properties Value Comments
Color Yellow to Brown
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved