Mallard Creek Polymers Tykote® 1019 Styrene-Butadiene Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name TYKOTE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Tykote® 1019 Styrene-Butadiene Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tykote® 1019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent film strength properties. It is intended for use as a base polymer in the formulation of barrier coatings for paper and paperboard packaging. Tykote® 1019 imparts excellent water resistance, and has good adhesion to a wide variety of surfaces. Tykote® 1019 is recommended for use in paper and paperboard coatings where a high degree of water and water vapor resistance is needed. It may also be formulated into barrier laminating adhesives for paper-to-paper, paper-to-film, and foil-to-paper. Regulartory Status: FDA components in food contact applications.175.105 indirect food additives176.170 components of paper and paperboard in contact with aqueous and fatty foods176.180 components of paper and paperboard in contact with dry food Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Tykote® 1019 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 52 - 54 %
52 - 54 %
Particle Size 0.18 µm
0.18 µm
pH 7.0 - 8.0
7.0 - 8.0
Brookfield Viscosity 150 - 850 cP
150 - 850 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 14.0 °C
57.2 °F
Descriptive Properties Value Comments
Emulsifiers Anionic