Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Microthene® F FN51000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Microthene® F
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Microthene® F FN51000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene F powders combine the unique properties of a polyolefin resin with a microfine particle size. Materials may contain flow-enhancing agents as required for processing and handling. Contact your Equistar sales and/or technical service representative for more information and specific recommendations for your application.Process TechniquesThe microfine size and spherical shape of Microthene F powders facilitate dispersibility in aqueous or organic systems. Specific suggestions can be made only when equipment, materials, process parameters and conditions of use are known. Contact your Equistar technical representative for more information. Regulatory StatusMicrothene powders comply with certain Food and Drug Administration regulations, which may or may not permit their contact with food. Specific limitations or conditions of use may apply. Contact your Equistar Regulatory Affairs representative for more information. This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.9225 g/cc
0.03333 lb/in³
ASTM D1505
Particle Size 5.0 - 50 µm
5.0 - 50 µm
Spherical shape, 5-50 micron distribution. ETM = Equistar Test Method; ETM Malvern
Maximum Moisture Content 0.10
0.10
ETM 156
Melt Flow 4.7 g/10 min
4.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.276 GPa
40.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
ASTM D3418
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525
Brittleness Temperature -76.0 °C
-105 °F
ASTM D746