Mallard Creek Polymers ROVENE® 4848 SBR Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 4848 SBR Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ROVENE® 4848 is a new developmental polymer specifically designed to be used in two part spray adhesives for open or closed cell foams and other contact and cold seal applications. Fast breaking characteristics may allow its use in specially formulated one part spray adhesives. When working with ROVENE® 4848 it is important to remember that it may be tackified, thickened, and blended with other carboxylated and non-carboxylated emulsions. It may also be blended with polychloroprene and natural latex if properly formulated. This flexibility allows for the formulating of a wide variety of adhesives with custom performance properties.APPLICATION: ROVENE® 4848 has found applications in two part foam-to-foam, one and two part fast breaking spray up adhesives, and special contact or cold seal applications in combination with polychloroprene and natural latex.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 52 - 54 %
52 - 54 %
Particle Size 0.17 µm
0.17 µm
pH 11 - 12
11 - 12
Brookfield Viscosity 200 - 800 cP
200 - 800 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
Chemical Properties Metric English Comments
Styrene Content 40 %
40 %
Descriptive Properties Value Comments
Emulsifiers Rosin Acid Soap