Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs TI550 (NH4)2TiF6 Ammonium hexafluorotitanate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs TI550 (NH4)2TiF6 Ammonium hexafluorotitanate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 197.95 g/mol
197.95 g/mol
Descriptive Properties Value Comments
Assay 24% Ti
CAS Number 16962-40-6
Form White crystals
Purity 99.998%
Typical Impurities Si = 10; Al = 3; Ca, Mg, Fe < 1 ppm
Users viewing this material also viewed the following: