Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Paratherm Corporation Paratherm™ CR Heat Transfer Fluid

Category Fluid
Manufacturer Paratherm Corporation
Trade Name Paratherm™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Paratherm Corporation Paratherm™ CR Heat Transfer Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet is capable of maintenance free operation up to 218°C (425°F). Applications include Fine and specialty chemical processing, pharmaceutical production, and environmental test chambersInformation provided by Paratherm Corporation.
Physical Properties Metric English Comments
Density 0.635 g/cc
<br>@Temperature 218 °C
0.0229 lb/in³
<br>@Temperature 425 °F
0.671 g/cc
<br>@Temperature 177 °C
0.0242 lb/in³
<br>@Temperature 350 °F
0.731 g/cc
<br>@Temperature 121 °C
0.0264 lb/in³
<br>@Temperature 250 °F
0.779 g/cc
<br>@Temperature 65.6 °C
0.0281 lb/in³
<br>@Temperature 150 °F
0.815 g/cc
<br>@Temperature 23.9 °C
0.0294 lb/in³
<br>@Temperature 75.0 °F
0.827 g/cc
<br>@Temperature 15.6 °C
0.0299 lb/in³
<br>@Temperature 60.0 °F
0.875 g/cc
<br>@Temperature -17.8 °C
0.0316 lb/in³
<br>@Temperature 0.000 °F
0.887 g/cc
<br>@Temperature -45.6 °C
0.0320 lb/in³
<br>@Temperature -50.0 °F
0.923 g/cc
<br>@Temperature -73.3 °C
0.0333 lb/in³
<br>@Temperature -100 °F
Viscosity 0.24 cP
<br>@Temperature 218 °C
0.24 cP
<br>@Temperature 425 °F
0.28 cP
<br>@Temperature 177 °C
0.28 cP
<br>@Temperature 350 °F
0.35 cP
<br>@Temperature 121 °C
0.35 cP
<br>@Temperature 250 °F
0.51 cP
<br>@Temperature 65.6 °C
0.51 cP
<br>@Temperature 150 °F
1.0 cP
<br>@Temperature -17.8 °C
1.0 cP
<br>@Temperature 0.000 °F
1.0 cP
<br>@Temperature 23.9 °C
1.0 cP
<br>@Temperature 75.0 °F
2.0 cP
<br>@Temperature -45.6 °C
2.0 cP
<br>@Temperature -50.0 °F
5.0 cP
<br>@Temperature -73.3 °C
5.0 cP
<br>@Temperature -100 °F
Viscosity Measure 0.38 cSt
<br>@Temperature 218 °C
0.38 cSt
<br>@Temperature 425 °F
0.42 cSt
<br>@Temperature 177 °C
0.42 cSt
<br>@Temperature 350 °F
0.48 cSt
<br>@Temperature 121 °C
0.48 cSt
<br>@Temperature 250 °F
0.65 cSt
<br>@Temperature 65.6 °C
0.65 cSt
<br>@Temperature 150 °F
0.94 cSt
<br>@Temperature 23.9 °C
0.94 cSt
<br>@Temperature 75.0 °F
1.5 cSt
<br>@Temperature -17.8 °C
1.5 cSt
<br>@Temperature 0.000 °F
2.5 cSt
<br>@Temperature -45.6 °C
2.5 cSt
<br>@Temperature -50.0 °F
5.5 cSt
<br>@Temperature -73.3 °C
5.5 cSt
<br>@Temperature -100 °F
Molecular Weight 130 g/mol
130 g/mol
average
Vapor Pressure 0.0373 bar
<br>@Temperature 65.6 °C
28.0 torr
<br>@Temperature 150 °F
0.277 bar
<br>@Temperature 121 °C
208 torr
<br>@Temperature 250 °F
0.959 bar
<br>@Temperature 177 °C
719 torr
<br>@Temperature 350 °F
1.432 bar
<br>@Temperature 218 °C
1074 torr
<br>@Temperature 425 °F
Thermal Properties Metric English Comments
Heat of Vaporization 344 J/g
148 BTU/lb
Specific Heat Capacity 1.59 J/g-°C
<br>@Temperature -73.3 °C
0.380 BTU/lb-°F
<br>@Temperature -100 °F
1.67 J/g-°C
<br>@Temperature -45.6 °C
0.400 BTU/lb-°F
<br>@Temperature -50.0 °F
1.80 J/g-°C
<br>@Temperature -17.8 °C
0.430 BTU/lb-°F
<br>@Temperature 0.000 °F
1.92 J/g-°C
<br>@Temperature 23.9 °C
0.460 BTU/lb-°F
<br>@Temperature 75.0 °F
2.09 J/g-°C
<br>@Temperature 65.6 °C
0.500 BTU/lb-°F
<br>@Temperature 150 °F
2.30 J/g-°C
<br>@Temperature 121 °C
0.550 BTU/lb-°F
<br>@Temperature 250 °F
2.51 J/g-°C
<br>@Temperature 177 °C
0.600 BTU/lb-°F
<br>@Temperature 350 °F
2.64 J/g-°C
<br>@Temperature 218 °C
0.630 BTU/lb-°F
<br>@Temperature 425 °F
Thermal Conductivity 0.125 W/m-K
<br>@Temperature 218 °C
0.864 BTU-in/hr-ft²-°F
<br>@Temperature 425 °F
0.128 W/m-K
<br>@Temperature 177 °C
0.888 BTU-in/hr-ft²-°F
<br>@Temperature 350 °F
0.133 W/m-K
<br>@Temperature 121 °C
0.924 BTU-in/hr-ft²-°F
<br>@Temperature 250 °F
0.137 W/m-K
<br>@Temperature 65.6 °C
0.948 BTU-in/hr-ft²-°F
<br>@Temperature 150 °F
0.140 W/m-K
<br>@Temperature 23.9 °C
0.972 BTU-in/hr-ft²-°F
<br>@Temperature 75.0 °F
0.144 W/m-K
<br>@Temperature -17.8 °C
0.996 BTU-in/hr-ft²-°F
<br>@Temperature 0.000 °F
0.1453 W/m-K
<br>@Temperature -45.6 °C
1.008 BTU-in/hr-ft²-°F
<br>@Temperature -50.0 °F
0.147 W/m-K
<br>@Temperature -73.3 °C
1.02 BTU-in/hr-ft²-°F
<br>@Temperature -100 °F
Boiling Point 182 °C
360 °F
Maximum Service Temperature, Air 218 °C
425 °F
288 °C
550 °F
max. recommended film temperature
Minimum Service Temperature, Air -88.3 °C
-127 °F
Flash Point >= 40.0 °C
>= 104 °F
closed cup; ASTM D56
Electrical Properties Metric English Comments
Volume Resistivity 8.3e+11 ohm-cm
8.3e+11 ohm-cm
Dielectric Constant 2.59
<br>@Frequency 1000 Hz
2.59
<br>@Frequency 1000 Hz
ASTM D924-04
Dielectric Breakdown 36110 V
<br>@Thickness 2.54 mm
36110 V
<br>@Thickness 0.100 in
ASTM D1816-04
Dissipation Factor 0.00145
<br>@Frequency 1000 Hz
0.00145
<br>@Frequency 1000 Hz
ASTM D924-04
Descriptive Properties Value Comments
Appearance water white
Autoignition >430°F
&lt; 10 sec delay
Chemistry synthetic hydrocarbon blend
Odor sweet