Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs NB800 Nb2O5 Niobium(V) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NB800 Nb2O5 Niobium(V) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 265.81 g/mol
265.81 g/mol
Descriptive Properties Value Comments
Assay 70% Nb
CAS Number 1313-96-8
Form White powder
Purity 99.999%
Typical Impurities Ta = 10; Si < 5; Ca = 3, Al = 1 ppm