Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 278.02 g/mol
278.02 g/mol
Descriptive Properties Value Comments
Assay 20% Fe
CAS Number 7782-63-0
Form Green crystals
Purity 99.999%
Typical Impurities Check with Manufacturer