Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite

Category Ceramic , Carbide , Metal , Metal Matrix Composite
Manufacturer M Cubed Technologies, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High stiffness, low density, low CTE composite. Components can be formed with complicated features, and can be machined to tight tolerances. Applications in high-precision equipment--semiconductor, automotive, aerospace.Information provided by M Cubed Technologies, Inc.
Physical Properties Metric English Comments
Density 3.01 g/cc
0.109 lb/in³
ASTM C135
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 230 MPa
33400 psi
ASTM E8
Modulus of Elasticity 270 GPa
39200 ksi
ASTM E494
Flexural Strength 230 MPa
33400 psi
ASTM C1161
Poissons Ratio 0.22
0.22
ASTM E494
Fracture Toughness 10.0 MPa-m½
9.10 ksi-in½
ASTM C1421
Shear Modulus 111 GPa
16100 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 6.20 µm/m-°C

@Temperature 25.0 - 100 °C
3.44 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
Thermal Conductivity 170 W/m-K
1180 BTU-in/hr-ft²-°F
ASTM E1461
Descriptive Properties Value Comments
Matrix Al Alloy
Particle Reinforcement SiC
Vol. % Reinforcement 70