Cotronics Resbond™ 950 High Temperature Ceramic Adhesive, Aluminum Composition

Category Ceramic
Manufacturer Cotronics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Resbond™ 950 High Temperature Ceramic Adhesive, Aluminum Composition.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mechanical Properties Metric English Comments
Flexural Strength 20.7 MPa
3000 psi
Compressive Strength 34.5 MPa
5000 psi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 6.34 W/m-K
44.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 649 °C
1200 °F