Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA860241 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA860241 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excellent balance of toughness, softness, dimensional stability and processability. Regulatory StatusNA 860 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 860 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2280
Tensile Strength at Break 8.48 MPa
1230 psi
Crosshead Speed - 20 in/min; ASTM D638
Tensile Strength, Yield 12.2 MPa
1770 psi
Crosshead Speed - 20 in/min; ASTM D638
Elongation at Yield 14 %
14 %
Crosshead Speed - 20 in/min; ASTM D638
1% Secant Modulus 221 MPa
32000 psi
Crosshead Speed - 1/2 in/min; ASTM D790
2% Secant Modulus 0.179 GPa
26.0 ksi
Crosshead Speed - 1/2 in/min; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Brittleness Temperature -35.0 °C
-31.0 °F
F<sub>50</sub>, Test method has been found useful for specification purposes, but does not necessarily indicate the lowest temperature at which the material may be used.; ASTM D746
Descriptive Properties Value Comments
Antioxidant Low
Slip High
Users viewing this material also viewed the following: