LyondellBasell Petrothene® NA814000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA814000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE NA 814-000 is a low density homopolymer resin specifically developed for a wide variety of blow molding applications. This resin exhibits excellent gloss, an excellent balance of physical properties and good processability. Regulatory StatusNA 814-000 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 814-000 has been specifically designed to provide excellent processability and flow properties, yielding improved output rates and part appearance. This resin can be molded over a wide range of melt temperatures with a recommended range of 350°-500°F. Specific recommendations for conditions under which NA 814-000 should be processed can be made only when the end use and type of processing equipment are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.9185 g/cc
0.03318 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 0.228 GPa
33.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C
104 °F
ASTM D648
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746