Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shrink film, shrink bundling, pallet shrink film, frozen food packaging, overwraps and heavy duty films where clarity and stiffness are important. Regulatory Status: The basic resin L3035 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for further information regarding the suitability of specific products for specific applications.Specific recommendations for the processing of L3035 can be made only when the end use application, required properties and the processing equipment are known. For exact recommendations, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
base resin; ASTM D1558
Thickness 50.8 microns
2.00 mil
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 14.5 MPa
2100 psi
ASTM D882
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
Film Elongation at Break, MD 470 %
470 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Impact Test 1.80 J
1.33 ft-lb
puncture strength; ASTM D5748
Elmendorf Tear Strength MD 230 g
230 g
ASTM D1922
Elmendorf Tear Strength TD 310 g
310 g
ASTM D1922
Film Tensile Strength at Break, MD 32.4 MPa
4700 psi
ASTM D882
Film Tensile Strength at Break, TD 28.3 MPa
4100 psi
ASTM D882
1% Secant Modulus, MD 303 MPa
44000 psi
ASTM E111
1% Secant Modulus, TD 338 MPa
49000 psi
ASTM E111
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 70 %
70 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 210 °C
410 °F
Die Opening 0.1524 cm
0.06000 in
Blow-up Ratio (BUR) 3.0
3.0
Copyright © lookpolymers.com All Rights Reserved