LyondellBasell Montell 12C01G5 Clarity LLDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer LyondellBasell
Trade Name Montell
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Montell 12C01G5 Clarity LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockApplications: food and non-food packaging, lamination films, coextruded structuresMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: 12C01 clarity LLDPE film resin combine ease of processing with excellent optics and high film strength. These resins are well suited to replace LLDPE/LDPE blends in blown film applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirmnets of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
ASTM D792
Thickness 25.4 microns
1.00 mil
Melt Flow 0.95 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.95 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.4 MPa
1800 psi
ASTM D882
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
Secant Modulus, TD 0.193 GPa
28.0 ksi
ASTM D882
Elmendorf Tear Strength MD 100 g
100 g
ASTM D1922A
Elmendorf Tear Strength TD 460 g
460 g
ASTM D1922A
Elmendorf Tear Strength, MD 3.94 g/micron
100 g/mil
ASTM D1922A
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
Dart Drop 3.94 g/micron
100 g/mil
ASTM D1709
Dart Drop Test 100 g
0.221 lb
ASTM D1709A
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
Film Tensile Strength at Break, TD 31.0 MPa
4500 psi
ASTM D882
Optical Properties Metric English Comments
Gloss 70 - 80 %
70 - 80 %
at 45°; ASTM D523
Transmission, Visible 90 %
90 %
clear; thickness not quantified