Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell DEXFLEX® 940 TPO

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name DEXFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell DEXFLEX® 940 TPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: DEXFLEX® 940 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior painted applications. Applications: Bumper fascias, claddings Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ISO 1183
Melt Flow 18 g/10 min
18 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.2 MPa
2930 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.413 GPa
204.9 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 17.5 J
12.9 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 85.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
47.2 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Users viewing this material also viewed the following: