Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SMAC CABLE® 2524S-30-08 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name CABLE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC CABLE® 2524S-30-08 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloy Screws: Inox A2Threaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 1398 daN
30.0 mm, up
315.0 daN
98.0 mm, 45° down and out
408.0 daN
58.0 mm, left and right
438.0 daN
54.3 mm, up and down
530.0 daN
65.0 mm, down
F, Max Static 134.0 daN
21.0 mm, 45° down and out
178.0 daN
11.5 mm, down
178.0 daN
8.0 mm, up
89.0 daN
20.0 mm, up and down
89.0 daN
23.0 mm, left and right
Transmissibility at resonance 3