Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Silvabraze 33830 Brazing Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name Silvabraze
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Silvabraze 33830 Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Silvabraze is used for brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten, and molybdenum. It is primarily used for the joining of copper-to-copper on vibration free joints. It is very effective for joining tight fitting copper pipe and tubing. Silvabraze should not be used on ferrous metals or copper alloys containing more than 10% nickel because of phosphorus embitterment due to reactions with iron or nickel. Silvabraze is extremely fluid at brazing temperatures and will penetrate joint with little clearance.Applications:The phosphorous content of Silvabraze acts as a fluxing agent and no flux is necessary when brazing copper to copper joints. However, when used with a copper alloy or one of the other brazeable metals, a brazing flux must be used to promote wetting, bonding, and flow throughout the joint.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.805 g/cc
8.805 g/cc
Density 8.08 g/cc
0.292 lb/in³
Thermal Properties Metric English Comments
Melting Point 643 - 821 °C
1190 - 1510 °F
Solidus 643 °C
1190 °F
Liquidus 821 °C
1510 °F
Maximum Service Temperature, Air 149 °C
300 °F
continuous
204 °C
400 °F
intermittent
Component Elements Properties Metric English Comments
Copper, Cu 92.3 - 93.25 %
92.3 - 93.25 %
As balance
Other, total <= 0.15 %
<= 0.15 %
Phosphorous, P 5.8 - 6.2 %
5.8 - 6.2 %
Silver, Ag 0.80 - 1.2 %
0.80 - 1.2 %
Tin, Sn 0.15 %
0.15 %
Processing Properties Metric English Comments
Processing Temperature 732 - 843 °C
1350 - 1550 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Copper
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved