Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt BRAZE 603 Silver Based Cadmium Free Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name BRAZE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt BRAZE 603 Silver Based Cadmium Free Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Braze 604 is a low temperature, low vapor pressure brazing filler metal formulated to meet the need for a composition free from volatile constituents, particularly essential in the brazing of vacuum tubes. The tin content of this filler metal improves its wetting characteristics on ferrous alloys over that obtainable with binary silver-copper filler metals. The tin addition also lowers the melting range versus binary silver-copper compositions. There is some tendency for the filler metal to liquate, but this is minimized by rapid heating to brazing temperature. Applications: Braze 603 is a silver-base brazing metal useful for making low temperature seals on vacuum tube components and for controlled atmosphere brazing of ferrous and non-ferrous alloys without flux. These filler metals are also recommended for brazing marine heat exchangers that are in contact with salt water, where there is a danger of dezincification to alloys containing zinc, particularly with joints on copper-nickel tubing. Specifications:This filler metals conform to the following specifications: AWS A5.8 BAg-18, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.82 g/cc
0.355 lb/in³
Thermal Properties Metric English Comments
Melting Point 601.7 - 718.3 °C
1115 - 1325 °F
Solidus 601.7 °C
1115 °F
Melting Point
Liquidus 718.3 °C
1325 °F
Flow Point
Component Elements Properties Metric English Comments
Copper, Cu >= 28.35 %
>= 28.35 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 59 - 61 %
59 - 61 %
Tin, Sn 9.5 - 10.5 %
9.5 - 10.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000241 ohm-cm
0.0000241 ohm-cm
Descriptive Properties Value Comments
Color White