| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 210 °C | 410 °F | |
| Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
| Zone 1 | 210 °C | 410 °F | Cylinder |
| Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
| Zone 1 | 210 °C | 410 °F | Cylinder |
| Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Zone 1 | 210 °C | 410 °F | Die |
| Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Zone 1 | 210 °C | 410 °F | |
| Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
| Zone 1 | 210 - 250 °C | 410 - 482 °F | |
| Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
| Zone 1 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 1 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 1 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 1 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
| Zone 1 | 210 °C | 410 °F | |
| Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
| Zone 1 | 210 - 230 °C | 410 - 446 °F | |
| Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
| Zone 1 | 210 °C | 410 °F | Injection Molding |
| UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||