Lord Adhesives Metech 3270 Silver Conductor

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lord Adhesives
Trade Name Metech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Metech 3270 Silver Conductor.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This composition is a silver bearing paste designed for screen print application of a fired conductive electrode. It forms a highly adherent bond to many compositions including alumina. The paste has good rheological properties and long screen life. The film has good initial and aged adhesion and is readily solderable.All information provided by Lord.
Physical Properties Metric English Comments
Brookfield Viscosity 90000 - 110000 cP

@Temperature 25.0 °C
90000 - 110000 cP

@Temperature 77.0 °F
RVT, Spindle #7 @ 20rpm
Component Elements Properties Metric English Comments
Silver, Ag 70 %
70 %
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.0025 ohm
<= 0.0025 ohm
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 25.0 °C
6.00 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Adhesion >4.4
lbs; Adhesion pad size 0.10"x0.10", solder 62Sn/36Pb/2Ag at 200ºC, 20 gauge pre-tinned copper wire at 90º to substrate plane.
Solder Wetting (seconds) 2-3
62Sn/36Pb/2Ag at 230ºC