Lord Adhesives Flocklok® 7000/7204 Flock Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Flocklok®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Flocklok® 7000/7204 Flock Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, nylon and ABS substrates.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.8747 - 0.8927 g/cc
0.03160 - 0.03225 lb/in³
7000 Adhesive
0.9287 - 0.9766 g/cc
0.03355 - 0.03528 lb/in³
7204 Cross-linker
Solids Content 13.5 - 16.5 %
13.5 - 16.5 %
7204 Cross-linker
29 - 31 %
29 - 31 %
7000 Adhesive
Brookfield Viscosity 15 cP

@Temperature 25.0 °C
15 cP

@Temperature 77.0 °F
7204 Cross-linker; LVT, Spindle #1 @ 100rpm
970 - 2500 cP

@Temperature 25.0 °C
970 - 2500 cP

@Temperature 77.0 °F
7000 Adhesive; LVT, Spindle #3 @ 30rpm
Thermal Properties Metric English Comments
Flash Point -5.00 °C
23.0 °F
7000 Adhesive; Seta
27.0 °C
80.6 °F
7204 Cross-linker; Seta
Processing Properties Metric English Comments
Cure Time >= 3.00 min

@Temperature 135 °C
>= 0.0500 hour

@Temperature 275 °F
on-line cycle
10.0 min

@Temperature 93.0 °C
0.167 hour

@Temperature 199 °F
off-line cycle
Shelf Life 6.00 Month

@Temperature 21.0 - 27.0 °C
6.00 Month

@Temperature 69.8 - 80.6 °F
7204 Cross-linker
12.0 Month

@Temperature 21.0 - 27.0 °C
12.0 Month

@Temperature 69.8 - 80.6 °F
7000 Adhesive
Descriptive Properties Value Comments
Appearance Clear, Amber-colored liquid
Solvents MEK
7000 Adhesive
Xylene, Acetates
7204 Cross-linker