Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Deloro® 60 Nickel Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Deloro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Deloro® 60 Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DELORO® 60 is a hardfacing alloy for application by welding and the Spray-fuse and powder-weld processes and in the form of castings, giving abrasion and corrosion resistant deposits. It can be ground, but is not machinable. DELORO® 60 has a very hard dense corrosion resistant coating with superior fusing characteristics.Information provided by Kennametal Stellite™
Mechanical Properties Metric English Comments
Hardness, Rockwell C 57 - 62
57 - 62
Component Elements Properties Metric English Comments
Boron, B 3.1 %
3.1 %
Carbon, C 0.70 %
0.70 %
Chromium, Cr 15 %
15 %
Iron, Fe 4.0 %
4.0 %
Nickel, Ni >= 72.8 %
>= 72.8 %
as balance
Silicon, Si 4.4 %
4.4 %
Descriptive Properties Value Comments
Application Technique HVOF & thermal spray
PTA & laser deposition
Spray-fuse & powder welding