Karina E 811-40/312-IS-RG Green PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 811-40/312-IS-RG Green PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.37 g/cc
1.31 - 1.37 g/cc
ASTM D 792
ASTM Color -10.95 - -4.95
-10.95 - -4.95
Color A, ME 12
11.03 - 17.03
11.03 - 17.03
Color B, ME 12
75.34 - 81.34
75.34 - 81.34
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application Alcoholic Beverage Bottles