Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 4980 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E800-18/258-CR-AS Gray PVC Compound
UV resistant PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
NBR NM-IEC 60811-1-1
Karina E810-40/312-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E818-10/23-CRM White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 801-10/88-CR White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 802-06/795-CRM Blue PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 811-10/9-Y-CRB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 830-21/9-IS-RG Coke PVC Compound
Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 830-42/16-IS-RG Red PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 830-48/1-IS-RG Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 835-42/14-IS-RG Red PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 850-10/199-Y-ERYM White PVC Compound
White PVC compound recommended for windows and profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 852-39/156-IS-RG Pink PVC Compound
Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 852-40/5-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina 861-40/28-IS-RG Green PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 750-35/2-IS-SD-TR-LMP Ivory PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 800-10/194-Y-CRB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 800-35/1-Y-CRB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 811-40/312-IS-RG Green PVC Compound
Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 817-48/1-F-ERYBT Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 818-10/23-CRM-AS White PVC Compound
UV. protection addedInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 820-10/1-D-TR White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 830-18/99-CRM Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 839-10/19-Y-CR White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 846-10/189-IS-SD White PVC Compound
Packaging Grade PVCInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 854-18/99-CRB Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 34.3 MPa
4980 psi
Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 34.3 MPa
4980 psi
Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 840-10/176-CRA White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 856-10/189-IS-SD White PVC Compound
White PVC compound recommended for extrusion of laminated/Sheet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Karina E 843-18/302-CRM Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Copyright © lookpolymers.com All Rights Reserved