Karina 924D10/349-IS White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina 924D10/349-IS White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.31 g/cc
1.25 - 1.31 g/cc
ASTM D 792
ASTM Color -1.72 - 0.28
-1.72 - 0.28
Color A, ME 12
-1.63 - 0.37
-1.63 - 0.37
Color B, ME 12
93.44 - 95.44
93.44 - 95.44
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 94

@Time 15.0 sec
90 - 94

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles