Karina 801-18/489-C-IS Gray PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina 801-18/489-C-IS Gray PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
ASTM Color -1.28 - 0.32
-1.28 - 0.32
Color A, ME 12
-0.120 - 1.48
-0.120 - 1.48
Color B, ME 12
70.05 - 71.65
70.05 - 71.65
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 12.6 MPa
>= 1820 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts
Technical Flexible Parts