GEHR Plastics POM-ELS Acetal, Electrically Conductive

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer GEHR Plastics Inc
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF GEHR Plastics POM-ELS Acetal, Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear because of the high strength and smooth surface. There is a very low risk of stress cracks. POM-C exhibits a high thermal stability and a high resistance to chemicals. Improved electrical conductivity.Properties:no microporosityhigh strengthhigh rigidityhigh thermal stabilitylow water absorptionhigh dimension stabilitygood electrical insulating propertiesvery good sliding propertieshigh resistance to stress cracksnot resistant to high concentrated acidsdifficult to glue and paintApplications include bearings, fittings, gear wheels, parts for pumps, screws, bobbins, parts for textile industry, and medium for coating lines.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 18 %
18 %
ISO 527
Elongation at Yield 7.0 %
7.0 %
ISO 527
Modulus of Elasticity 2.00 GPa
290 ksi
ISO 527
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ISO 75
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 10 ohm-cm
<= 10 ohm-cm
VDE 0303
Surface Resistivity per Square <= 1000 ohm
<= 1000 ohm
VDE 0303
Descriptive Properties Value Comments
Acid Resistance no
Bondability no
Color Black
Physiological indifference according no
UV Stabilization no