Johnson Matthey Mattibraze 50N Silver Brazing Alloy for Tungsten Carbide Brazing

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Mattibraze 50N Silver Brazing Alloy for Tungsten Carbide Brazing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A cadmium containing alloy for brazing tungsten carbides, beryllium copper, and aluminum bronze to steel. Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. The localized extraction of fumes during brazing is now virtually obligatory. The use of cadmium containing alloys is not permitted in the manufacture of food and drink handling equipment and medical instruments. If cadmium containing alloys are felt likely to cause a health hazard then use a cadmium free alloy from the Johnson Matthey Matti-sil range. Full details on exposure levels (OES) are given in the specific Material Safety Data Sheets. These should always be consulted before use of a cadmium bearing brazing alloy.Optimum Joint Gap 0.1 - 0.25 mm.AMS 4771AWS A5.8-92 BAg-3BS EN 1044 1999 AG351Federal Specification QQ-B-564 VEquivalent to Engelhard Silvaloy 50NEquivalent to Handy & Harman Easy-flo 3Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 634 - 656 °C
1170 - 1210 °F
Solidus 634 °C
1170 °F
Liquidus 656 °C
1210 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 16 %
16 %
Copper, Cu 15.5 %
15.5 %
Nickel, Ni 3.0 %
3.0 %
Silver, Ag 50 %
50 %
Zinc, Zn 15.5 %
15.5 %