TOOLOX 33 is a quenched and tempered tool steel designed to have low residual stresses and extremely good machinability. Applications include: Plastic molds; Rubber molds; Bending tools; Machine componentsTesting in accordance with EN 10 137-1, 10 137-2 and EN ISO 6506-1. Hardness measured on a milled surface, 0,5-2 mm below surface.Information provided by International Mold Steel
Mechanical Properties Metric English Comments
Hardness, Brinell 280 - 330
280 - 330
Hardness, Rockwell C 30 - 35
30 - 35
Tensile Strength 896 - 979 MPa
130000 - 142000 psi
Charpy Impact, Unnotched 100 - 180 J
74.0 - 133 ft-lb