Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that require good see-through clarity combined with good heat resistance and refrigerator temperature impact properties can benefit from the use of grade R01C-00. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsThermoformed packaging (cups, containers, lidding) Extrusion blow molded containers and bottles Injection blow molded containers and bottles Extruded sheet and profilesBenefitsExcellent clarity Excellent processability Good impact resistance at room and refrigerator temperatures Low static charge
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.6 MPa
4150 psi
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% Secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 5.23 J/cm

@Diameter 3.17 mm
9.80 ft-lb/in

@Diameter 0.125 in
bar; Hinge Failure; ASTM D256
0.747 J/cm

@Diameter 3.17 mm,
Temperature 4.00 °C
1.40 ft-lb/in

@Diameter 0.125 in,
Temperature 39.2 °F
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
ASTM D648
Optical Properties Metric English Comments
Haze 11 %

@Thickness 1.27 mm
11 %

@Thickness 0.0500 in
plaque; ASTM D1003
Descriptive Properties Value Comments
Process Blow Molding
Extrusion
Injection Molding
Thermoforming
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved