Proto3000 Objet Digital Materials™ DM_9610 Rubber-like Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Proto3000 Objet Digital Materials™ DM_9610 Rubber-like Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primary material: TangoGraySecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85
75 - 85
ASTM D2240
Tensile Strength at Break 9.00 - 13.0 MPa
1310 - 1890 psi
ASTM D412
Elongation at Break 45 - 55 %
45 - 55 %
ASTM D412
Tear Strength 44.1 - 49.0 kN/m
252 - 280 pli
ASTM D624